The pressure cowling is formed by first installing the baffle, covering
with plastic, and filling with liquid foam. |
|
The foam is trimmed and sanded to the desired shape. The upper
cowling should be trial fit to ensure adequate clearance. Once the
desired shape is obtained the mold is used to form the pressure cowl. |
|
The final result is shown here. |